Drying Physically fast drying,dries at 20℃ within 20 to 30 min.(for overprintability),at 50℃ in a tunnel dryer within 30-60sec.The times mentioned vary according to thickness of the ink film,with or without addition of hardener and type of hardener,drying conditions and auxiliaries used.Please note that the drying speed slows down i shades are overprinted and a hardener has been used. Stress resistance After proper and thorough drying,the ink film exhibits outstanding adhesion as well as rub and scratch resistance and is resistant to oils,greases,diluted acids and bases,and alcohol. |